Nb: SrTiO3 (100), 0.5 wt% Nb, 10x10x0.5mm, 1sp (Crystal Made in Japan) - STONba101005S1JPdop05US

Nb: SrTiO3 (100), 0.5 wt% Nb, 10x10x0.5mm, 1sp (Crystal Made in Japan) - STONba101005S1JPdop05US

RM0.00 MYR
Sale price  RM0.00 MYR Regular price 
Skip to product information
Nb: SrTiO3 (100), 0.5 wt% Nb, 10x10x0.5mm, 1sp (Crystal Made in Japan) - STONba101005S1JPdop05US

Nb: SrTiO3 (100), 0.5 wt% Nb, 10x10x0.5mm, 1sp (Crystal Made in Japan) - STONba101005S1JPdop05US

SKU: stonba101005s1jpdop05us

Price: RFQ

Description

Single crystal SrTiO3 Nb-doped 0.5 wt% Size: 10mm x 10mm x 0.5mm Orientation: (100)  +/-0.5 o Polish: one side polished. Surface finish( RMS or Ra): <5A Typical Physical Properties Crystal Structure Cubic, a=3.905 A Nb doping 0.5 wt% Growth Method Vernuil Density 5.175 g/cm 3 Melt Point 2080 o C Hardness 6 ( Mohn) Thermal expansion 10.4 (x10 -6 / o C) Resistivity 0.003 ~ 0.007 ohm.cm for 0.5 wt% Nb doped SrTiO3 (If you would like to measure the resistivity accurately, please order our Portable 4 Probe Resistivity Testing Instrument .) Loss Tangent at 10 GHz ~5x10 -4 @ 300K , ~3 x10 -4 @77K Color and Appearance Black Chemical Stability Insoluble in water Customers Who Bought This Item Also Bought: SrTiO3 LSAT LaAlO3 MgO Film Coaters Portable 4 Probe Resistivity Tes te r SrLaAlO4 NdCaAlO4 NdGaO3 YSZ Wafer Boxes Plasma/UO Cleaner

 

Typical Physical Properties

Crystal Structure

Cubic, a=3.905 A

 Nb doping  0.5 wt% 

Growth Method

Vernuil

Density

5.175 g/cm3

Melt Point

2080 oC

Hardness

6 ( Mohn)

Thermal expansion

10.4 (x10-6/ oC)

Resistivity

0.003 ~ 0.007 ohm.cm for 0.5 wt% Nb doped SrTiO3
(If you would like to measure the resistivity accurately, please order our Portable 4 Probe Resistivity Testing Instrument.)

Loss Tangent at 10 GHz

~5x10-4 @ 300K , ~3 x10-4 @77K

Color and Appearance

Black

Chemical Stability

Insoluble in water

,
     